TECHNET Archives

May 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 24 May 2012 15:29:00 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Ioan Tempea <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
Dear Technos,

 

What is your experience with wave soldering of 0.031" thick boards? Is it possible to pass them without wave pallets, with leading and trailing stiffeners only?

 

I'm still trying to figure out the panel, guess it will be something like 7"x11".

 

Thanks,

 

Ioan Tempea

Ingénieur principal de fabrication / Senior Manufacturing Engineer

  <http://www.digico.cc/> 

 

950 RUE BERGAR, LAVAL, QC, H7L 5A1 <http://g.co/maps/2gh3f> 

T+ 1 (450) 967-7100, EXT244

------------------------------------------------------------------------

    <http://www.facebook.com/pages/Digico/277076778479> 

------------------------------------------------------------------------

Lauréat Dunamis 2012 <http://digico.cc/dunamis-2012/> 

Entreprise manufacturière / Gestion du capital humain

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2