Technetters,
I have a simple question.
Does anyone know what the wetting angles of the two phases of the Pb-Sn eutectic on a Au surface are.
Or at least which one is lower?
Any direct answer (number/reference) will be greatly appreciated.
Regards,
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca