TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 5 Apr 2012 09:51:12 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (81 lines)
Agreed.  I believe Richard is referring to the seldom referenced Vapidus 
temperature where vapor and liquid can co-exist.

Doug Pauls



From:   "Fox, Ian" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   04/05/2012 09:26 AM
Subject:        Re: [TN] Max time above liquidus
Sent by:        TechNet <[log in to unmask]>



Richard, the liquidus temperature is the maximum temperature at which 
solid crystals can co-exist with liquid. Above the liquidus the material 
is completely liquid. The solidus temperature is in contrast the 
temperature below which liquid can't exist. In terms of a tin/lead phase 
diagram it is the upper boundary of the liquid+solid "mushy" region

Regards
Ian

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 05 April 2012 14:32
To: [log in to unmask]
Subject: Re: [TN] Max time above liquidus

You mean time above solidus. Time above liquidus is vapor. 
Yes, 105 degrees in liquidus does seem excessive, but it depends on the 
size/mass of the CCA being soldered. It might be required for very large 
CCAs.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fabien Guizelin
Sent: Wednesday, April 04, 2012 6:04 PM
To: [log in to unmask]
Subject: [TN] Max time above liquidus

Hi,
Should I be concerned by excessive TAL ?   (inter-metalic, etc)
Do you consider 105sec TAL with a Indium 5.1 paste excessive ?   (Indium 
recommends 45-60sec)
Thanks,
Fabien



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.

______________________________________________________________________
Aero Engine Controls is a trading name of Rolls-Royce Goodrich Engine 
Control Systems Limited, Registered office Moor Lane Derby DE24 8BJ 
Registered number 6686268, registered in England

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2