Can you build with 2 oz power and 2 oz ground on the same core?. If you can run half ounce signal planes together on the next core - great.
-----Original Message-----
From: Ravinder.Ajmani <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Thu, Apr 26, 2012 8:19 pm
Subject: Re: [TN] Core with uneven Copper foil thickness
Hi All,
Thanks to all who have responded. Perhaps I should add that this is a
2-layer PCB, and the 2 oz Copper layer will be used for Power/Ground
nly. The signal layers will be 1/2 oz thick.
egards
avinder Ajmani
rincipal HW Engineer, Signal Integrity / EMI
GST, a Western Digital company
[log in to unmask]
"Lehmicke, Michael" <[log in to unmask]>
ent by: TechNet <[log in to unmask]>
4/26/2012 02:57 PM
lease respond to
echNet E-Mail Forum <[log in to unmask]>; Please respond to
Lehmicke, Michael" <[log in to unmask]>
o
[log in to unmask]>
c
Subject
e: [TN] Core with uneven Copper foil thickness
avinder;
Although uneven copper thicknesses on a core are more common that one
ould expect, 1/2 oz. versus 2 oz. can cause some issues during the
tching process, depending on trace pitch and tolerances. One would need
o see the gerber files to determine if it would be an issue.
There are ways to get around this issue on Multilayer flex, but if this is
ust a double layer flex it has to be addressed. There are techniques,
sing a combination of additive/subtractive processes, to build up
hickness during processing on just one side. Again, the trace widths and
olerances can influence this type of processing.
Mike Lehmicke
olex Copper Flex products
2 Empire Drive
t. Paul, MN 55103
51-846-7728
[log in to unmask]
----Original Message-----
rom: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
ent: Thursday, April 26, 2012 4:40 PM
o: [log in to unmask]
ubject: [TN] Core with uneven Copper foil thickness
Hi,
We are considering a layer stackup which uses Cores with uneven Copper
oil thickness. Copper on one side is 1/2 oz and on the other side is 2
z. Apart from the availability/cost considerations are there other
ssues with using such a Core.
I will appreciate the opinions of experts on this.
Thanks.
egards
avinder Ajmani
rincipal HW Engineer, Signal Integrity / EMI
GST, a Western Digital company
[log in to unmask]
______________________________________________________________________
his email has been scanned by the Symantec Email Security.cloud service.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
ONFIDENTIALITY NOTICE: This message (including any attachments) may
ontain Molex confidential information, protected by law. If this message
s confidential, forwarding it to individuals, other than those with a
eed to know, without the permission of the sender, is prohibited.
This message is also intended for a specific individual. If you are not
he intended recipient, you should delete this message and are hereby
otified that any disclosure, copying, or distribution of this message or
aking of any action based upon it, is strictly prohibited.
English | Chinese | Japanese
ww.molex.com/confidentiality.html
_____________________________________________________________________
his email has been scanned by the Symantec Email Security.cloud service.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
______________________________________________________________________
his email has been scanned by the Symantec Email Security.cloud service.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|