TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Thu, 5 Apr 2012 15:21:56 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Fox, Ian" <[log in to unmask]>
Message-ID:
Subject:
From:
"Fox, Ian" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (106 lines)
Yes he was. Liquidus and solidus are metallurgical terms which describe the upper and lower boundary lines of liquid+solid regions in alloy phase diagrams, in fact as they are also used in glass phase diagrams. Open any metallurgical text book and in the phase diagram section you will find them thus described.

It also sounds like Doug has been at the mountain dew again :-)

Regards
Ian

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 05 April 2012 15:59
To: [log in to unmask]
Subject: Re: [TN] Max time above liquidus

Werner emailed several times to me directly, and to others on the forum that the term "above liquidus" should not be used when dealing with eutectic solder, as there was no such thing as being above the liquidus, ie, above the molten state. The solder is liquidus above the solidus temperature, solid below it. So, to describe the molten state of the solder, the correct term would be "above solidus". Was he wrong?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, April 05, 2012 9:51 AM
To: [log in to unmask]
Subject: Re: [TN] Max time above liquidus

Agreed.  I believe Richard is referring to the seldom referenced Vapidus temperature where vapor and liquid can co-exist.

Doug Pauls



From:   "Fox, Ian" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   04/05/2012 09:26 AM
Subject:        Re: [TN] Max time above liquidus
Sent by:        TechNet <[log in to unmask]>



Richard, the liquidus temperature is the maximum temperature at which solid crystals can co-exist with liquid. Above the liquidus the material is completely liquid. The solidus temperature is in contrast the temperature below which liquid can't exist. In terms of a tin/lead phase diagram it is the upper boundary of the liquid+solid "mushy" region

Regards
Ian

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 05 April 2012 14:32
To: [log in to unmask]
Subject: Re: [TN] Max time above liquidus

You mean time above solidus. Time above liquidus is vapor. 
Yes, 105 degrees in liquidus does seem excessive, but it depends on the size/mass of the CCA being soldered. It might be required for very large CCAs.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fabien Guizelin
Sent: Wednesday, April 04, 2012 6:04 PM
To: [log in to unmask]
Subject: [TN] Max time above liquidus

Hi,
Should I be concerned by excessive TAL ?   (inter-metalic, etc)
Do you consider 105sec TAL with a Indium 5.1 paste excessive ?   (Indium 
recommends 45-60sec)
Thanks,
Fabien



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.

______________________________________________________________________
Aero Engine Controls is a trading name of Rolls-Royce Goodrich Engine Control Systems Limited, Registered office Moor Lane Derby DE24 8BJ Registered number 6686268, registered in England

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.

______________________________________________________________________
Aero Engine Controls is a trading name of Rolls-Royce Goodrich Engine Control Systems Limited, Registered office Moor Lane Derby DE24 8BJ Registered number 6686268, registered in England

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2