Agreed. I believe Richard is referring to the seldom referenced Vapidus
temperature where vapor and liquid can co-exist.
Doug Pauls
From: "Fox, Ian" <[log in to unmask]>
To: <[log in to unmask]>
Date: 04/05/2012 09:26 AM
Subject: Re: [TN] Max time above liquidus
Sent by: TechNet <[log in to unmask]>
Richard, the liquidus temperature is the maximum temperature at which
solid crystals can co-exist with liquid. Above the liquidus the material
is completely liquid. The solidus temperature is in contrast the
temperature below which liquid can't exist. In terms of a tin/lead phase
diagram it is the upper boundary of the liquid+solid "mushy" region
Regards
Ian
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 05 April 2012 14:32
To: [log in to unmask]
Subject: Re: [TN] Max time above liquidus
You mean time above solidus. Time above liquidus is vapor.
Yes, 105 degrees in liquidus does seem excessive, but it depends on the
size/mass of the CCA being soldered. It might be required for very large
CCAs.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fabien Guizelin
Sent: Wednesday, April 04, 2012 6:04 PM
To: [log in to unmask]
Subject: [TN] Max time above liquidus
Hi,
Should I be concerned by excessive TAL ? (inter-metalic, etc)
Do you consider 105sec TAL with a Indium 5.1 paste excessive ? (Indium
recommends 45-60sec)
Thanks,
Fabien
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
______________________________________________________________________
Aero Engine Controls is a trading name of Rolls-Royce Goodrich Engine
Control Systems Limited, Registered office Moor Lane Derby DE24 8BJ
Registered number 6686268, registered in England
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|