TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 4 Apr 2012 23:03:31 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Fabien Guizelin <[log in to unmask]>
Message-ID:
Subject:
From:
Fabien Guizelin <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (13 lines)
Hi,
Should I be concerned by excessive TAL ?   (inter-metalic, etc)
Do you consider 105sec TAL with a Indium 5.1 paste excessive ?   (Indium recommends 45-60sec)
Thanks,
Fabien



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2