TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Mon, 30 Apr 2012 17:39:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
<000001cd2719$ae65b860$0b312920$@com>
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (107 lines)
Hi Richard,

Yes we wash everything, DI water only, no chemistry. All of our paste,
fluxes, and core solder is water soluble.

I've looked at the boards post reflow but prior to cleaning and have not
noticed any mid-chip balls. 

I will look a little closer just to make sure, to see if maybe we're washing
them away. 

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, April 30, 2012 3:56 PM
To: [log in to unmask]
Subject: Re: [TN] Homeplates on 4 mil thick stencils?

Steve,
Somewhat related to the other discussion on cleaning of no-clean:
Do you wash the assemblies after reflow, and is that why you do not see any
mid-chip solder balls?
Do you wash any CCAs that have been processed with a no-clean solder paste
or no-clean wire solder?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, April 30, 2012 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] Homeplates on 4 mil thick stencils?

BTW I forgot to add I don't homeplate anything...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, April 30, 2012 3:16 PM
To: [log in to unmask]
Subject: Re: [TN] Homeplates on 4 mil thick stencils?

Hi Ioan,

We use 4-mil thick stencils quite often and I don't see mid-chip balling...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, April 30, 2012 2:54 PM
To: [log in to unmask]
Subject: [TN] Homeplates on 4 mil thick stencils?

Dear Technos,

 

It is my first 4 mil stencil and I was wondering if mid-chip balling is
still an issue at this thickness (no-clean process). Should I still
homeplate the apertures of passives, as I fear insufficient solder?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T |
450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W |
www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2