TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Julie Silk <[log in to unmask]>
Date:
Thu, 26 Apr 2012 19:47:22 -0400
Message-ID:
Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
Subject:
From:
Robert Kondner <[log in to unmask]>
X-cc:
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (25 lines)
Julie,

 Ok, Dollars to Doughnuts. Let's say I get some of the Kester 985M. What is the easiest way to test if heat deactivation is required?

 As someone who ran a wave machine for years I know darn well that there is a lot of flux that never gets near the wave. The foam and spray systems will get flux up on ICs and into connectors, everywhere. Preheaters I have used were always facing only the board bottom.

 I am going to follow up with Kester. I still question how much "Deactivation" can be accomplished with heat as so much flux goes into so many places. I still cannot believe this stuff requires heating to be as good as indicated on the data sheet, but I could be wrong. I think it comes in pens, I will get one.

Thanks again for your time.
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
Sent: Thursday, April 26, 2012 7:25 PM
To: [log in to unmask]
Subject: Re: [TN] 4 Questions: No Clean vs flux Deactivation. Possible Hogwash ???

The wave solder will deactivate the acids in this liquid wave-solder flux (and in my last message I meant to say deactivate the flux, not deactivate the solder!), so unless the flux gets sprayed in a place where it won't see a decent amount of heat, there's no issue with this flux.  Yes, it can leave a mess, but usually it's a thin layer of flux residue that is hard and not tacky, and has a high SIR.  When used in the right process!  I also like the clean look of watersoluble fluxed boards, but there are times when these will get trapped under low/no clearance parts and cause leakage paths.  Also, there are certain parts that can't tolerate exposure to halide-containing acid fluxes, so those need a different flux selection.  Another way-back experience was with RMA flux residues during a harsh condensing test -- it acted like a conformal coating, preventing the metal from shorting under condensation.  Wouldn't be a guarantee, but it decreased the shorting, didn't increase it.  


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2