The mean at 245 degreeC (230 to 260)with +10oC, it should show a PMI of +67%, PMI will depend on your setting. Thus you must know what is your needed process control
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Mack
Sent: Wednesday, 28 March 2012 1:06 AM
To: [log in to unmask]
Subject: Re: [TN] PWI for reflow
The leading profile datalogger companies sell pallets to run through the
oven. They have built in thermocouples and magnets used to sense conveyor
speed. Their software has basic SPC software included that collects data
for you, and an easy go/no-go display for the machine operator.
Run the pallet once a week, day or shift on the same program and you will
get measurements to confirm the oven remains stable.
This is a very capable method to catch bad heaters, fans, changes in
exhaust,,,
Roger Mack P.Eng.
Manufacturing Specialist
Parker Hannifin Canada
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB R3T 1T4 Canada
direct 204 453 3339 x373
[log in to unmask]
www.parker.com/ecd
From:
Fabien Guizelin <[log in to unmask]>
To:
<[log in to unmask]>
Date:
03-27-2012 03:28 AM
Subject:
[TN] PWI for reflow
Sent by:
TechNet <[log in to unmask]>
Hello,
Could you give me guideline on how to set-up PWI limits for SMT ?
I experienced a +10oC drift in max-temperature on a transformer between a
profile taken a year ago and recently. I am concerned about the
potential impact it has on the component (over-temperature).
My CM currently operates at 230-260C peak-temp range which seems broad;
how does this compares to industry best-practices ?
Thanks for the help.
Fabien
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
"PLEASE NOTE: The preceding information may be confidential or
privileged. It only should be used or disseminated for the purpose
of conducting business with Parker. If you are not an intended
recipient, please notify the sender by replying to this message and
then delete the information from your system. Thank you for your
cooperation."
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|