Being retired, I still do some jobs for a SPACE company. We have a routine
for incoming components named 'Forbidden material'. 100% of the incoming
components are inspected and checked in a XRF machine. When I say 100%,
there are of course excemptions : we fo not test all screws in a batch of 5
thousand.
Inge
----- Original Message -----
From: "David D. Hillman" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, March 20, 2012 11:14 PM
Subject: Re: [TN] Out of the world tin whiskers
> Hi Pat and gang - good information as our "industry attention" on the
> topic of tin whiskers pre-1997 was not at the same level of scrutiny as we
> have today. This failure, if it has a tin whisker root cause, is a
> demonstration of two things: (1) the breakdown of system rules prohibiting
> the use of pure tin in a space application. NASA has always attempted to
> avoid the use of pure tin due to the tin whisker risk. There may have been
> a simple human error or this could have been a lack of knowledge by a
> supplier; (2) the lack of a tin whisker mitigation strategy. If there was
> going to be the use of pure tin in a space application, was a tin whisker
> mitigation methodology missed - such as pretinning the leads, adequate
> design spacing or the use of a coating material to capture/contain the
> whiskers? Easy to second guess what happened. Hopefully, further details
> of the story will be published so that we can learn from the issue.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
>
>
> "Goodyear, Patrick" <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 03/20/2012 02:33 PM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
> "Goodyear, Patrick" <[log in to unmask]>
>
>
> To
> <[log in to unmask]>
> cc
>
> Subject
> Re: [TN] Out of the world tin whiskers
>
>
>
>
>
>
> To answer my own question.
>
> Cassini was launched October 15,1997, so it was most likely built in
> '96-'97 timeframe. I don't think lead free had hit the streets by then
> except for applications in plumbing. Whiskers had been an issue long
> before that, at least in my industry. We have been inspecting for them
> since around 1992, we tripped a unit in 1988 due to a whisker in a relay,
> shorting out a contact that should have opened when the relay energized.
>
> pat
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
> Sent: Tuesday, March 20, 2012 11:11 AM
> To: [log in to unmask]
> Subject: Re: [TN] Out of the world tin whiskers
>
> But Cassini is a bunch of years old, at least 10 I think. The components
> are most likely plated leads on diodes or tin canned pots.
>
> Pat
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Dale Ritzen
> Sent: Tuesday, March 20, 2012 11:00 AM
> To: [log in to unmask]
> Subject: Re: [TN] Out of the world tin whiskers
>
> Joyce,
> I know your question below is basically rhetorical, but have you tried to
> find a component without a Pb-free coating on it lately... That is,
> unfortunately, why there are Pb-free components on spacecraft... and
> obviously tin whiskers.
>
> Dale Ritzen, CQA
> Quality Manager / ISO Management Representative Austin Manufacturing
> Services
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
> Sent: Tuesday, March 20, 2012 12:57 PM
> To: [log in to unmask]
> Subject: Re: [TN] Out of the world tin whiskers
>
> I thought space is exempt for leadfree. Why?
> --------------------------
> Sent using BlackBerry
>
>
> ----- Original Message -----
> From: Inge Hernefjord [mailto:[log in to unmask]]
> Sent: Tuesday, March 20, 2012 01:47 PM
> To: [log in to unmask] <[log in to unmask]>
> Subject: Re: [TN] Out of the world tin whiskers
>
> DO THEY NEVER LEARN!
>
> Inge
>
> On 20 March 2012 18:08, Gervascio, Thomas L
> <[log in to unmask]>wrote:
>
>> Tin whiskers at Saturn
>>
>> PASADENA, Calif. -- The Cassini plasma spectrometer instrument (CAPS)
>> aboard NASA's Cassini spacecraft at Saturn has resumed operations.
>> Mission managers received confirmation on Friday, March 16, that it was
> turned on.
>> They plan to monitor the instrument for any unusual behavior.
>> Last June, short circuits in the instrument led to unexpected voltage
>> shifts on the spacecraft. As a precaution, mission managers turned off
>> the CAPS instrument while engineers investigated the issue. The
>> investigation led to the conclusion that tin plating on electronics
>> components had grown "whiskers." The whiskers were very small, less
>> than the diameter of a human hair, but they were big enough to contact
>> another conducting surface and carry electrical current. Researchers
>> are still trying to understand why whiskers grow on tin and other
>> metals, but they know now that whiskers can grow in space and on
>> Earth. It is believed that these or additional tin whiskers that may
>> grow on Cassini cannot carry enough current to cause problems, but will
> burn out on their own like a lightweight fuse.
>>
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud
> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute non-public
> information. Any use of this information by anyone other than the intended
> recipient is prohibited. If you have received this transmission in error,
> please immediately reply to the sender and delete this information from
> your system. Use, dissemination, distribution, or reproduction of this
> transmission by unintended recipients is not authorized and may be
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|