I don't know NASA's routines. European satellites use to be run for x hs
before launching, It's done in order to cut the familiar early failures in
the start of the 'bath tub ' curve. Maybe, whiskers do not grow so
fast in these tests as being in the orbit.
/Inge
On 23 March 2012 15:36, Bob Landman <[log in to unmask]> wrote:
> Steve,
>
> I asked Henning about a satellite that failed in orbit due to whiskers as
> to how they could possibly deduce that when I saw him at the CALCE meeting
> at UMd. He told me it was because they had similar equipment on the ground
> and could verify that whiskers had likely erupted.
>
> Bob
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
> Sent: Thursday, March 22, 2012 4:50 AM
> To: [log in to unmask]
> Subject: Re: [TN] Out of the world tin whiskers
>
> Bob,
>
> Yes, will be very interesting to hear what the group can share.
>
> Could it be possible they still have a back-up/alternate CAPS instrument/s
> in storage to physically examine for whiskers, thereby making the problem
> definition a bit easier.
>
>
> Steve C
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|