TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 8 Mar 2012 20:18:50 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Goodyear, Patrick" <[log in to unmask]>
Message-ID:
Subject:
From:
"Goodyear, Patrick" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<E448D2D184D44A13996662BDCFC9E69A@stephenPC>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (49 lines)
They were attached will do it again.
p 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, March 08, 2012 11:25 AM
To: [log in to unmask]
Subject: Re: [TN] Black substance

Hi Pat,

Reply to me with the pictures and I'll get them posted...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Thursday, March 08, 2012 1:39 PM
To: [log in to unmask]
Subject: [TN] Black substance

Ok got a new one.    Found on the plated portion of a turret a black fuzz,
also on the riveted backside and the plated portions of all of the lands outside the soldered areas.
It cleans right off with alcohol leaves no residue, is crystalline in structure and grows away from the metal has a coral like appearance.

I have attached pictures but Steve is off today so don't know who else can post.

Again a 40 year old board.

Any ideas????

Pat

.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2