TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Goodyear, Patrick" <[log in to unmask]>
Date:
Thu, 8 Mar 2012 17:02:35 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (57 lines)
Hi Pat - what are/is the plating layers on the turrets? Silver? I assume 
the solder is tin/lead.

Dave



"Goodyear, Patrick" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
03/08/2012 12:39 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Goodyear, Patrick"     <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Black substance






Ok got a new one.    Found on the plated portion of a turret a black fuzz, 
also on the riveted backside and the plated portions of all of the lands 
outside the soldered areas.
It cleans right off with alcohol leaves no residue, is crystalline in 
structure and grows away from the metal has a coral like appearance.

I have attached pictures but Steve is off today so don't know who else can 
post.

Again a 40 year old board.

Any ideas????

Pat

.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2