They were attached will do it again.
p
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, March 08, 2012 11:25 AM
To: [log in to unmask]
Subject: Re: [TN] Black substance
Hi Pat,
Reply to me with the pictures and I'll get them posted...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Thursday, March 08, 2012 1:39 PM
To: [log in to unmask]
Subject: [TN] Black substance
Ok got a new one. Found on the plated portion of a turret a black fuzz,
also on the riveted backside and the plated portions of all of the lands outside the soldered areas.
It cleans right off with alcohol leaves no residue, is crystalline in structure and grows away from the metal has a coral like appearance.
I have attached pictures but Steve is off today so don't know who else can post.
Again a 40 year old board.
Any ideas????
Pat
.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|