TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Dennis Fritz <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 6 Mar 2012 11:05:23 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, harvey <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (67 lines)
Now I know why I make so many soft errors. I'm radioactive!
Anyhow, we're doling our best to "eliminate" solder, period.
As an opportunist, I welcomed Mahendra's question.

Flip Chips will be replaced by BBUL and embedded KGD constructions.
That is a better solution than SAC.




________________________________
From: Dennis Fritz <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, March 6, 2012 10:41:55 AM
Subject: Re: [TN] Fw: Help. Is this true-- SOFT ERRORS FROM SOLDER??

Harvey, 

Lead is the decomposition product of uranium - over millions/billions of years.  
Alpha free lead has been sought for many years for the bumps on IC chips, where 
alpha particles could upset semiconductor gates.  However, most anything stops 
an alpha particle, so Pb in solder joints on a board are usually pretty far away 
from the silicon itself.  The IBM C4 chip attach technology uses/used 95% lead 
material so the IC bumps wouldn't melt during board assembly with 63/37. Pre 
1945 lead is prized because it has not picked up radioactive stuff from nuclear 
testing (makes you feel good about what we breathe and eat).  Anyway, lead 
ballast from old ships (back to Roman days) is one of the best sources of alpha 
free lead. 


SAC solder should not shed alpha particles, and is another reason IBM and others 
are looking to take C4 process to Pb-free.

Denny



-----Original Message-----
From: harvey <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Tue, Mar 6, 2012 11:58 am
Subject: [TN] Fw: Help. Is this true-- SOFT ERRORS FROM SOLDER??


Could this be true only of 63-37 or would lead-free SAC alloys also be  
potentially guilty of causing soft errors?    ----- Forwarded Message ---- From: 
"Gandhi, Mahendra S (AS)" <[log in to unmask]> To: 
"[log in to unmask]" <[log in to unmask]>;  
"[log in to unmask]" <[log in to unmask]>;  
"[log in to unmask]" <[log in to unmask]> Sent: Tue, March 6, 2012 
8:38:40 AM Subject: Help. Is this true??    Evidently regular solder has 
decaying Uranium in it, or somehow generates alpha  particles, which are being 
blamed for upsets.  Some chips are moving to a  special “low alpha” solder 
internally to avoid this problem on bump-grid-arrays  in  flipchip parts.    
Mahendra Gandhi SME - PWB Technologies Aerospace Engineering One Space Park, 
M5/1085A Redondo Beach, Ca. 90278/*[log in to unmask] (Office: 310.813.6857 
Fax: 310.812.8630   
______________________________________________________________________ This 
email has been scanned by the Symantec Email Security.cloud service. For more 
information please contact helpdesk at x2960 or [log in to unmask]  
______________________________________________________________________ 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2