Hi Dieter,
If it possible, I will appreciate sending me the C version of 7095 for
review. I have lot of experience with the BGAs mix technology process and
have my own work process and profile temperature instructions so I can give
my remarks to the committee.
Reuven
On Sun, Mar 4, 2012 at 7:31 PM, Dieter Bergman <[log in to unmask]>wrote:
> Dear Raye,
>
> We are in the process of completing the "C" revision of IPC-7095. The
> topic in which you expressed an interest will be in the new document.
>
> I've attached the minutes of the telephone call last year in which this
> topic was reviewed and we agreed to add the explanations to the table as
> shown in the minutes. That information should give you some good advice and
> characterize the reflow profile that is recommended for the situation.
>
> I've just returned from the APEX meeting in San Diego and although we are
> in the Balloting process we have a few additional Technical comments that
> were resolved at the meeting. These comments were about adding some more
> information on the causes of voids in the solder joint. We have to go for
> another short circulation to get the committee approval before we publish.
> There were no additional comments on the section that references table 7-3.
>
> I hope this helps.
>
> Best regards,
>
> Dieter
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Rivera, Raye
> Sent: Thursday, March 01, 2012 2:11 PM
> To: Technet
> Subject: [TN] BGA Reverse Backwards Compatibility
>
> Hello TechNet Gurus.
>
> I have seen lots of discussion and studies on the reliability of using
> BGAs with SAC solder balls on an assembly with SnPb paste. Many people are
> interested in this topic because of backwards compatibility issues when
> SnPb BGAs aren't available. At the risk of oversimplifying a complex topic,
> I understand this can be successful using a backward compatibility thermal
> profile such as the one shown on Figure 8-20 of IPC-7095B to ensure
> complete melting of both types of solder. Of course we must take care that
> the profile does not exceed the temperature limitations of the SnPb paste.
>
> Is anyone aware of any study done on the reverse situation? That is, SnPb
> BGAs used with SAC solder paste and a SAC thermal profile? I would think it
> would be at least as reliable as the above situation. We definitely get
> complete melting and the temperature profile is correct for the SAC solder
> paste chemistry so we are not as concerned about holding a narrow process
> window.
>
> This is not just academic curiosity on my part. We have some prototype
> boards built with SnPb BGAs SAC paste, and SAC profile. They are not for
> sale to customers, but some of our engineers are of the opinion that any
> mixed process joint is suspect. I'd like to find some data on the topic.
>
> I hope everyone is enjoying Apex.
>
> Best regards,
> Raye Rivera
>
> QA Manager * Canoga Perkins
> 20600 Prairie Street * Chatsworth * CA 91311-6008
> 818-678-3872 * [log in to unmask]
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
--
Best Regards,
*Reuven Rokah*
Mobile: 972-52-60-120-18
Tele-fax: 97239360688
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com
**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|