You mean other than "once you try it, you're stuck with it"?
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, March 12, 2012 8:39 AM
To: [log in to unmask]
Subject: [TN] Assembling with conductive adhesive
Hey all,
Wish I hadn't lost that hour of sleep this weekend, I'll try to find it
tonight. :o)
Anyways, have any of you thought of trying to replace solder with a
conductive adhesive for PCB assembly? There's a few out there (Henkel,
Cookson, Ellsworth, etc.) that are touting them as solder replacements.
When I read the technical datasheets, I'm thinking to myself, why isn't this
stuff more widely used? There must be a reason.
I do know it's pretty expensive almost all of them are silver filled, and I
have read that the mechanical strength and thermal conductivity is not as
good as solder, but what other reasons are out there not to use it?
Steve
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|