Re: [TN] looking for suggestions for no-clean flux-core PB-free wire
solder
Julie Silk
to:
TechNet
02/27/2012 11:21 AM
Sent by:
TechNet <[log in to unmask]>
Please respond to TechNet E-Mail Forum, Julie Silk
You are handsoldering through hole, so you will want a wire diameter that
will give you a good amount of solder in a small amount of time. While you
want thin wire (.010-.015") for SMT, you want thicker for TH, but I'm not
sure of the exact diameter (.025-040?). SAC 305, 2-3% flux so you get good
wetting. We use Alpha Telecore Plus or Kester 275, maybe others. Just a
note, the lead-free solder is not lead-free. It usually has a Pb content
betwee 300 and 700 ppm.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________