Hi Stewart - I would recommend that before you launch into a SAC305 copper
dissolution project that you investigate the published data as there has
been a tremendous volume of work in that area already. Sources in my
references include:
- a number of papers presented in the IPC APEX and SMTAI conferences in
the 2005-2012 time frame
- NPL (Dr. Chris Hunt and team) did a great study on dissolution rate
- Craig Hamilton and the folks from Celestica have some great publications
on copper dissolution
- the NASA DoD report has copper dissolution data for SAC305 and SN100C
solder alloys (the report is on the web)
Your question on "how thick can IMC get before we have cracking issues" is
a good question but the reality is that the number of IMC cracking issues
published can be counted on one hand. Using industry typical soldering
process, either tin/lead or leadfree solder alloys, you need to severely
abuse the process parameters to get into those types of situations.
Published data by Thwaites and Klein Wassink covers the IMC topic. There
is no IPC standards on copper dissolution or IMC thickness that I am aware
of.
Good luck with the effort.
Dave Hillman
Rockwell Collins
[log in to unmask]
Stewart McCracken <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/02/2012 04:11 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Stewart McCracken <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
[TN] Cu - dissolution and IMC growth rate
Fellow Technetters,
We are going to be involved in a project this year looking at rates of Cu
dissolution and IMC layer growth during soldering processes (including
rework).
At this stage, I would like to ask the wider community whether anybody has
or knows of "rules of thumb", or published data etc. which describes rates
of dissolution and rates of IMC layer growth?
A little more specifically, based on a SAC305 alloy system, and using an
Immersion Silver or OSP PCB finish, we are looking to develop our
understanding of the following points:
1. IMC growth (microns) for SAC305 solder as a function of time exposure
(seconds) above 230C
2. Cu dissolution (microns) for SAC305 solder as a function of time
exposure (seconds) above 217C
3. Does anyone work to a defined critical threshold (in terms of max IMC
thickness) above which PCB functional integrity is considered to be
undermined?
4. Does anyone work to a defined critical threshold (in terms of min Cu
thickness) below which PCB functional integrity is considered to be
undermined?
5. Are there IPC or other standards covering these items?
I would be extremely grateful for your input, and would be very happy to
share results of the experimental programme which we will undertake later
this year.
Thanks and kind regards,
Stewart
Stewart McCracken
MCS Ltd.
Centre House
Midlothian Innovation Centre
Roslin
Midlothian
EH25 9RE
U.K.
t. +44 (0)131 440 9090
m. +44(0)7711 541735
e. [log in to unmask]
w. www.themcsgroup.co.uk
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|