TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Julie Silk <[log in to unmask]>
Date:
Mon, 27 Feb 2012 16:31:41 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Fox, Ian" <[log in to unmask]>
Message-ID:
Subject:
From:
"Fox, Ian" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (21 lines)
For the purposes of the RoHS legislation a solder (or any other homogeneous material for that matter) is considered lead free if the lead composition is determined to be below 0.1wt%

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
Sent: 27 February 2012 16:21
To: [log in to unmask]
Subject: Re: [TN] looking for suggestions for no-clean flux-core PB-free wire solder

You are handsoldering through hole, so you will want a wire diameter that will give you a good amount of solder in a small amount of time.  While you want thin wire (.010-.015") for SMT, you want thicker for TH, but I'm not sure of the exact diameter (.025-040?).  SAC 305, 2-3% flux so you get good wetting.  We use Alpha Telecore Plus or Kester 275, maybe others.  Just a note, the lead-free solder is not lead-free.  It usually has a Pb content betwee 300 and 700 ppm.  

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.

______________________________________________________________________
Aero Engine Controls is a trading name of Rolls-Royce Goodrich Engine Control Systems Limited, Registered office Moor Lane Derby DE24 8BJ Registered number 6686268, registered in England

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2