你好:IPC-610中就有相关规定,在E版的10-42页中,从图上看不出是否有粘性和潮湿等。所以你要自己看下
缺陷- 2,3级
* 助焊剂残留物妨碍目视检查。
* 助捍剂残留物妨碍接近组件的测试点。
* 潮湿、有粘性、或过多的助焊剂残留物,可能扩展到其他表面。
缺陷- 1,2,3级
* 在任何电气连接表面上阻碍电气连接的免洗助焊剂残留
物。
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Roger Liu
Sent: Wednesday, February 15, 2012 9:01 AM
To: [log in to unmask]
Subject: [TGAsia] Non-clean Flux Residue
(See attached file: Flux Residue2.pptx)
请教各位专家:
如图示,免清洗助焊剂残留是否可以接受?
如果不可以接受,请教应该引用什么标准来要求?
Best Regards!
Roger LIU / 刘芝新
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
Important:
This email is intended only for the person or entity to which it is addressed and may contain confidential and/or privileged material. Any disclosure, copying, distribution or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. If you have received this in error, please contact the sender immediately and delete the material from your systems. (C) 2012 Copyright Enics Group. All rights reserved.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|