请参考以下文件:
1.JEDEC/IPC-JP002 JEDEC/IPC Current Tin Whiskers Theory and Mitigation Practices Guideline
Scope:This document provides insight into the theory behind tin whisker formation as it is known today and, based on this knowledge, potential mitigation practices that may delay or prevent tin whisker formation. The potential effectiveness of various mitigation practices will also be briefly discussed. References behind each of the theories and mitigation practices are provided. Due to additional performance requirements, the mitigation methods in this document may not be sufficient for certain applications with special needs (e.g., military or aerospace).
2.JESD201 Environmental Acceptance Requirements for Tin Whisker Susceptibility of Tin and Tin Alloy Surface Finishes
3.JESD22A121 Measuring Whisker Growth on Tin and Tin Alloy Surface Finishes
Best regards,
张学良 Bliver Zhang
Technology Resources Coordinate 标准化协调
深圳市南山区南海大道新保辉大厦27楼 A-D
27F A-D, Xin Baohui Building, Nanhai Blvd, Nanshan District, Shenzhen
Tel: +86 755-86141218 / 86141219
Fax: +86 755-86141226
MP:15099906258
Email:[log in to unmask]
________________________________
发件人: TGAsia [[log in to unmask]] 代表 bo.xu [[log in to unmask]]
发送时间: 2012年2月9日 8:50
到: TGAsia
主题: [TGAsia] Tin Whisker锡须相关问题
大家好!
我想咨询一下, IPC中是否有Tin Whisker锡须的相关资料?
包括锡须的形成, 生长速率与工艺和环境的相关关系, 锡须实验的实验要求, 实验条件, 样品数量, 后续改善方法等, 谢谢!
现在我们需要做以下实验, 顺便请大家介绍下哪里可以做.
Tin Whisker Acceptance – 9 PWB assemblies are built up using production solder and attachment methods.
Assemblies need to be preconditioned and then inspected.
Assemblies are then split into three lots of three per JEDEC JESD201A table 4a. Inspections need to be recorded with SEM inspection. Preconditioning is required.
Stress Test Conditions Inspection Interval Test Duration
Temp/Cycling -40 to 85 C with 10 minute soak 500 Cycles 1500 Cycles
Temp/Humidity 30 C / 60% RH 1000 hours 4000 hours
High Temp/Humidity 55 C / 85% RH 1000 hours 4000 hours
Pass/Fail Criteria: – Less then 10 whiskers per 25 mm2 area. Maximum whisker length is shorter then the distance between any terminals on assemble.
2012-02-09
________________________________
Regards!
Bo Xu
工程技术部
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|