Carl, If the coating is in fact acrylic, the isopropyl alcohol will remove the coating without any degradation the component or board material. If it is something other than Acrylic coating, then take a look at the IPC document IPC-7711/7721 for specific removal processes. Hope this Helps, Peggi Blakley
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: Thursday, February 09, 2012 13:00
To: [log in to unmask]
Subject: [TN] How can I remove solder mask?
I have a PC board that somebody has repaired, and then painted something that looks like the standard green soldermask to cover the repair. There is still a short circuit under the painted area. I'd like to analyze the repair, but I don't want to just scrape off the covering with a knife blade. Is there an easily available solvent that can be used to remove soldermask?
Thanks,
Carl
p.s. I check the archives, and was unable to get any results with the search function. It seems to be broken . . .
Carl Van Wormer, P.E., AE7GD
Senior Hardware Engineer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Cipher Systems (503) 617-7447 x 5163
Direct Line (503) 425-5163
[log in to unmask]
This message may contain confidential and/or proprietary information, and is intended for the person/entity to whom it was originally addressed. Any use by others is strictly prohibited. If I sent this to you by mistake, please be nice and delete it, then tell me of my mistake so I can send it to the right person.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|