TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Sat, 4 Feb 2012 19:24:33 -0500
Reply-To:
Message-ID:
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (48 lines)
Hi,

 

I was reading through the Ellis book on cleaning and I noticed adding IPA to
water reduces surface tension. 

 

Neat, I figure that is a simple way to improve a rinse. I was planning on
final rinse with distilled water so I don't need to bother with blow off as
much.

 

Just for fun I looked into various grades and it looks like dissolved
materials is about .005% or 39mg / Liter. (1 L = 780gram)

 

Hmmmm, That sounds rather high compared to distilled water. I mean Lake
Michigan is 170 mg/L I think.

    (See:
http://www.aquapurefilters.com/contaminants/163/total-dissolved-solids.html)

 

No one would think twice about dipping a cleaning swap into IPA to clean a
board. But Lake Michigan water? Holy Cow!

 

Did I find the wrong specs on the IPA?

 

Bob K.

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2