Hey Victor!
Got your pictures, and they don't look too good:
http://stevezeva.homestead.com/DIMM_Contcat_corrosion-1.JPG
http://stevezeva.homestead.com/DIMM_Contact_with_corrosion-1a.JPG
I know that probably someone else that has seen this before will be able to
be more specific this appearance that I can...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, February 29, 2012 9:53 AM
To: [log in to unmask]
Subject: [TN] Field Return Product w/corrosion product
Fellow TechNetters;
Do No Clean LF fluxes, Rosin Core/molten solder, have a corrosive ion?
Every so often when conducting analysis on Field Return Product I notice
small amount of corrosion product on gold plated contact on DIMM and PCI
Slot connector. Sometimes on other gold plated connector leads. So I am
trying to understand which component had a corrosive ion waiting for the
right conditions to flourish. Small amount of greenish/bluish residue.
It can be seen on wipe zone and/or stamp edge of contact. Where is this
active corrosive ion coming from?
Can someone provide the link to Stevezea home page for posting pictures?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|