TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 22 Feb 2012 08:25:13 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Phil Bavaro <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (133 lines)
Perhaps a reverse home base plate design is needed.

I also wonder if you might be dealing with misprinted boards not being
cleaned adequately since it is random.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Wednesday, February 22, 2012 12:05 AM
To: [log in to unmask]
Subject: Re: [TN] Microballs

Hi Reuven,
Thanks for the answer.
See my  comments below

Best regards,

CANTAGALLO Luigi
Technology Engineer




Reuven Rokah <[log in to unmask]>
22/02/2012 07:52

A
TechNet E-Mail Forum <[log in to unmask]>,
[log in to unmask]
cc

Objet
Re: [TN] Microballs






Hi Luigi,
You have to check:
1. Size of pads (too long under the components body).
        On recurrent products, we use the same pads from years without
this problem 2. Size of opening in stencil
        Openings are the same with reduction of 20% of opening for R0805
and R1206. No reduction for capacitors 3. P&P accuracy
        Checked. It's OK and we have decreased the placing force (To not
crush the paste) without impact on the balls 4. Solder paste temperature
(should be room temperature)
        Checked. It's OK. And we have tested the solderability and
coalescence. The "old" paste lots are same quality the news.
5. Oxidation of component / PCB [ads / solder paste particles
        The PCB are checked. For the components we are checking if there
is a correlation between defect/PCB/components
 
Reuven


On Wed, Feb 22, 2012 at 8:33 AM,
<[log in to unmask]>
wrote:
Hello everybody.

Any  idea about random presence of microballs (diameter 0.1 to 0.5 mm)
beneath some chips (R and C 0805, 1206,1210, 1812) ?
We use a SnPb process with a vapor phase oven.
We use same types of PCB, same process on same SMT line in a clean room
from years and the balls are randomly present from some months now.
They could be present in one lot of PCB and not the following; beneath a
component on one PCB and not on the same component on other PCB; we have
balls one day and not the day after; the balls disappear for weeks and
re-appear after; ...
I have checked different lots of solder paste, origin of PCB's, all
parameters of printing, P&P and the cleaning (co-solvent station). The
thermal profiles are same.
As it's hi-rel production I cannot change easely products and process.
I suspect a process parameter but which ?
I ask myself if there is not a ghost in the line .. :-)

Best regards.

CANTAGALLO Luigi
Technology Engineer


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________



--
Best Regards,

Reuven Rokah 
   
Mobile: 972-52-60-120-18
Tele-fax: 97239360688
[log in to unmask]
[log in to unmask]
www.rokah-technologies.com


This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2