Hóla Victor,
is Hernandez your full name or is it followed by more, like Victor b Juarez
Bernardo Hernandez y Caballo de Montana Grosso de Asuncion. I have seen
some impressive names.
Well, there are many methods. Looked briefly through my zinc pile if there
was something for you. You hav
alkaline non-cyanide solutions
chloride solutions
Doctor's solution
Envirozin 2 non cyanide solution
Hylite 80
Unizin
Zincalux
etc
These are sometimes followed by passivation like
Blue passivation
Zinc chromate
Iridex
Zonax
Autopass salts
Black chromate
etc
With other words a jungle. I saw no correlation to whiskers, more than that
whiskers have been observed for a 'number of zinc platings'. Not much of a
help. The general advice to avoid whisker formation is to avoid baths that
produce interatomare tension (general, not only for zinc) . Therefore many
avoid brighteners and/or perform heat treatment. All that has been
presented on seminars for many years, but some go further and use
zero-whisker- formation-solutions. Like this one:
http://www.sambix.co.jp/english/zerowhisker.html. But there are more. This
was what I had. May give you a start. Hoping that someone with zinc finish
as specialty give you more. I know people in that discipline if noone
bites. With the limited knowledge I have, I vote for heat treatment in
first place, because passivation can fail locally. As a second I vote for a
'doped' zinc, but that, again, is for sharper guys to develop.
q.e.s.m.
Ingge
On 18 February 2012 20:01, Victor Hernandez <[log in to unmask]>wrote:
> Fellow TechNetters;
>
> I understand that there a several methods of plating zinc and that
> perhaps only one yield zinc whiskers. Can someone share their input with
> zinc plating. I have examined several zinc plating surfaces, sheet metal
> extrusions-chassis, without knowing their process and one has zinc
> whiskers. Is this a correct observation. I will request plating specs
> for each sample examined.
>
> Victor,
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|