If the CCA goes through any type of AOI post reflow, then have those holes added to the inspection. Almost any AOI machine can detect any unfilled holes.
Also, where is the requirement for the holes to be filled or checked in your process documentation? Is there an operation where the operator is told to verify holes are filled, and touchup if not? If they work/inspect off of the assembly print, can a print note be added?
Somewhere there needs to be a documented requirement that the holes be filled. Talking to a wave solder operator and trying to get him/her to "remember" this requirement is futile. They are busy remembering what they did last Friday night. Find a means to poka-yoke the process so the holes are always filled.
OR, if there is no other requirement to have any solder in those holes, leave the solder out of the holes and make a test fixture consisting of a 2x5 bed of solid nails embedded in a non-conductive material. Just plug it in when you test each board. The metal pins will seal each hole and provide electrical contact to the barrels, without shorting the barrels together. To more easily envision this, suppose you took a plastic table with ten metal legs, turned it upside down, and plugged it into the connector holes....except don't use plastic, use Durostone CAS 716, which is dissipative.
If you go that route, you just need to add the masking of the holes to the process so NO solder is added. A piece of Kapton tape will work, or peelable/soluble masking.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: Tuesday, January 24, 2012 1:01 PM
To: [log in to unmask]
Subject: [TN] Wave solder - filling of "empty" holes
We have a PCB assembly with a 2x5 pin "engineering" header that is not
populated on our production boards. The normal results of our CM's wave
solder process yields boards with the 10 holes (.040" dia.) filled with
solder. Our pointed spring-probe test fixture hits the centers of these
solder-filled holes, and all is good with the world . . .
Occasionally, we have some boards that do not have all of the holes
filled (I can provide a picture if it helps the discussion). The test
fixture spring-probes may penetrate into the unfilled holes, making only
intermittent contact with the hole-walls. My final solution may be to
obtain spring-probes with wider tips to bridge the hole, making contact
with the annular ring, but I'd like to get opinions from the group as to
my expectations of hole-filling in the wave solder process.
I'm sure that 10mil holes will always fill, and 1000mil holes, will
never fill. What expectations should I have with my 40mil holes (in my
62 mil thick PCB)? If the consensus is that the holes should fill, what
suggestions can I give to my CM to facilitate my desired hole filling?
Thanks,
Carl
Carl Van Wormer, P.E., AE7GD
Senior Hardware Engineer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Cipher Systems (503) 617-7447 x 5163
Direct Line (503) 425-5163
[log in to unmask] <mailto:[log in to unmask]>
This message may contain confidential and/or proprietary information,
and is intended for the person/entity to whom it was originally
addressed. Any use by others is strictly prohibited. If I sent this to
you by mistake, please be nice and delete it, then tell me of my mistake
so I can send it to the right person.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|