Thanks.
Tin, wherever used, may form whiskers.
The list of sources would include tin plating anywhere, lead free solder, and 63-37 solder.
But I believe that lead deters whisker formation in eutectic solder generally.
That is a statement that is supported by empirical history and much more.
I'm copying Carol Handwerker for her opinion on the subject.
--- On Mon, 1/23/12, Julie Silk <[log in to unmask]> wrote:
From: Julie Silk <[log in to unmask]>
Subject: Re: [TN] Finally, the folly of lead-free solder is making the big time
To: [log in to unmask]
Date: Monday, January 23, 2012, 8:10 AM
These weren't soldered with lead-free
solder. It was tin-lead. The problem was tin-plated parts or boards (maybe both?).
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For
additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|