You can re-certify expired solder paste per J-STD-005 section 6.0. Used the form attached therein, and follow the appropriate test methods (also listed at the end of J-STD-005, #2.4.34, 2.4.34.1, 2.4.34.2, 2.4.34.3 for the viscometer you wish to use. You should always perform first article testing, monitor your PPMO, etc., and document all product run with the re-certified paste.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juliano Pacheco
Sent: Monday, January 16, 2012 7:30 AM
To: [log in to unmask]
Subject: [TN] Expired Solder Paste
Hi,
What are the consequences of using expired solder paste?
How long after the expired date is "acceptable"?
Thank you.
Juliano Pacheco
|
|
|