In the past I've used Omegameter and Ionograph as process control after
washing process, always = 10 minutes.
To consider also instrument measurement method:
- Dynamic method
- Static method
(first minutes of test, the curves D-S may behave in a different way)
- Temperature of media 75/25
Regards
Gabriele
-----Messaggio originale-----
Da: TechNet [mailto:[log in to unmask]] Per conto di Garcia, Rigo
(GSFC-300.0)[MANTECH SRS TECHNOLOGIES]
Inviato: giovedì 26 gennaio 2012 17.16
A: [log in to unmask]
Oggetto: [TN] Typical ROSE Test Duration
Hi everybody!
I have looked at several document but can't find the answer. This should be
an easy one for my TechNet buddies though.
Does anybody know what the typical duration for the ROSE Test is?
Rigo Garcia
Sr. Quality Assurance Engineer
Workmanship Standards, Code 300
NASA, Goddard Space Flight Center
Greenbelt, MD 20771
Phone. (301) 286-6129
Fax. (301) 286-6576
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|