In fact, FEW chelates, which we would nominally call a "chelate", are toxic.
Of course the KING of chelates is EDTA, which is even administered as a drip into the blood stream. Others include Citric Acid, etc. NTA is a cheep version of EDTA, and has some health issues, but, frankly, if I were putttng together a hand wipe to remove Lead, I would use EDTA, and then recommend a water rinse. FYI.
Rudy Sedlak
RD Chemical Co.
--- On Thu, 1/12/12, Karen Tellefsen <[log in to unmask]> wrote:
From: Karen Tellefsen <[log in to unmask]>
Subject: Re: [TN] Hand Wipes and Lead Residues
To: [log in to unmask]
Date: Thursday, January 12, 2012, 9:03 AM
Not all chelating agents are toxic, though some are.
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
Re: [TN] Hand Wipes and Lead Residues
Amol Kane
to:
TechNet
01/12/2012
11:50 AM
Sent by:
TechNet <[log in to unmask]>
Please respond to TechNet E-Mail Forum, Amol Kane
Any wipe that cleans lead residues would have to have chelate on them. What
about any harmful effects of chelate due to skin contact? How do you clean
chelate off the hands?
We use chelate wipes to clean benches/work surfaces if absolutely needed,
but there is always a secondary wipe with alcohol involved to remove the
chelate
Amol Kane | Process Engineer
Catalyst Manufacturing Services, Inc.
941 Route 38, Owego NY 13827
Phone: (607) 687-7669 Extn 349 | Website: www.catalystems.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Thursday, January 12, 2012 11:31 AM
To: [log in to unmask]
Subject: Re: [TN] Hand Wipes and Lead Residues
Doug,
My still under-employed comments on the subject are:
1 - I can visualize how wipes may sanitize and/or de-oil the hands
somewhat;
2 and they may remove some lead residues;
3 but I don't see how a wipe could be as effective as a good wash with
running water and soap. I would be surprised if the wipe could keep
metallic residues in suspension without re-depositing on the skin somewhere
else.
Unfortunately, with soap and water, any metallic residue goes down the
drain and then where???
At least the wipes would likely be sequestered in a landfill somewhere.
Shortcuts are not always the best path to take.
On the other hand, if there is a barely detectable amount there in the
first
place, possibly the wipes will reduce it below the delectability threshold.
Steve Creswick
http://www.linkedin.com/in/stevencreswick
616 834 1883
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, January 12, 2012 11:03 AM
To: [log in to unmask]
Subject: [TN] Hand Wipes and Lead Residues
Good morning all,
I just had a chat with one of our ES&H engineers, a very pleasent young
lady, on the topic of hand wipes and lead residues. Was I aware of any
industry studies on the efficiency of hand wipes marketed at removing lead
residues, presumably from contact with cored wire solder? I was not aware
of any. I am always instantly suspicious of ANYTHING that marketers
touch. I am of the opinion that good old fashioned hand washing with soap
and water is as effective as anything, but there are areas here where we
are pretty sure our operators go straight from the bench to lunch without
that step.
So, I turn to my favorite source of information.
1. Are you aware of any industrial hygiene studies regarding
transferrence of lead to the hand, and/or the efficiency of "lead removal
wipes" in removing residues.
2. In your facilities, do you use these kinds of wipes?
3. If not, what measures do you normally use for operators cleaning hands
to remove potentially harmful material?
I will probably discuss this with our crackerjack metallurgist when he
returns from travel tomorrow, but thought I would ask in the mean time.
Doug Pauls
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|