I am in the process of getting this design changed but have another
question related to it:
This device data sheet does not have a recommended land pattern, only
the mechanical drawing for the part.
If the center slug on the part is 3.5 mm, shouldn't the pad on the board
be larger than 3.5?
My designer is saying that the IPC pad calculator is matching the size
exactly but this just doesn't sit right with me. It doesn't allow for
any tolerance of the size and I have always seen pad center slugs larger
than the component's slug.
I measured a part and found the actual size to be over 4 mm, and the
xray shows that inside the component, the heat spreader size is even
larger (almost 5 mm).
Thanks in advance,
Phil
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|