TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Date:
Mon, 9 Jan 2012 11:21:11 -0500
Reply-To:
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (258 lines)
Steve,

 Weight immediately after blow off and then immediately after drying. 

 We only need to get down to the .01g level is my expectation. 

 While I don't know the sensitivity your "Super Balance" it is probably MUCH better than the $6 unit I order and that is 0.01g. I suspect you were MUCH more sensitive. Round off to .01g is OK. If you can get a stable reading down to .001g that would be fantastic.

Bob

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Monday, January 09, 2012 11:10 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux‏

Bob,

I can not provide an answer, but have another issue.  The major issue I have with weighing for contamination is - "When".

I've had super-balances in the past where if one were to take a 'dry' object and place it on the balance you would see a continuous weight gain as moisture was re-ad/absorbed over a span of seconds, minutes and hours.

I did this with an unsealed hybrid [metal, ceramic, IC's adhesive], but would expect to see the re-gathering of moisture with a PWB even more substantially, and over a longer period of time.

Seems like weighing will forever be a fuzzy technique unless the 'when' variable can be suitably removed.

Is the test still valid if one's balance can not detect the re-ad/absorption of moisture from the room air?

Food for thought?

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of residuguru
Sent: Monday, January 09, 2012 10:21 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux‏

The amount of water trapped after blow off under components alone can be significant and I have a sensitive scale where we will weigh the samples. I will put together a matrix today and set a date that anyone that wants to visit during the experiment is invited.  I am going to use Kokomo tap water and I have Mckinney TX tap water as well.  Both we have well documented by Ion Chromatography.  We even have an Aquastorm 200 with great blowers that we will use as one of the varibles to remove the water residues.  We know that these blowers are good but not effective on drying from below components so that is why we use cross flow ovens to bake the boards dry at 85C for a couple of hours after cleaning.  I look forward to this evaluation.  I am planing on the sample processing to take place next Thursday Jan 19, 2012 at 10 am.  The amount of TDS is less important than the amount of corrosive ionic and organic residues that the water leaves behind.  I will also include the doping o  f FR-4 laminate electrodes and air blow off to determine the amount of residue left behind on a non solder masked areas of the boards. I have attached a paper on cleanliness testing of the Umpire 2 and the type of analytical approach we will perform. 

Terry Munson
Foresite
765-457-8095



In a message dated 01/09/12 09:44:55 Eastern Standard Time, [log in to unmask] writes:
Hi, Bob
I can assure you that the amount of water retained on a CCA after blow-off is very significant.
Water is trapped inside of connector bodies, underneath all flat components, and many other places that cannot be blown dry. Blowing boards with air may get most of the visible moisture off of the board, but leaves a lot of water behind. In addition, even a grounded blower unit can build up a charge of over 250 volts, enough to damage many ESD components. Blow-off is also somewhat expensive because it is time consuming and you need a pretty good compressor running almost at a 100% duty cycle. Also, almost all compressed air has some oil or other contaminants in the line.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, January 09, 2012 7:35 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux‏

Terry,

You pooh-pooh tap water but failed to state two important parameters:

 1. Dissolved content in tap water. Let's assume it is all ionic in nature. (500mg / L Seems like worst case)

 2. Amount of water that remains on a board (average per sq. inch) after blow off.

 I would love to see the results of a test as you propose. Let us not argue like CAD Monkeys, let us do an experiment.

I would ask that you weight the PCB after the final blow off of tap water and then after a hot air dry, the difference being retained tap water residue. I am very curious as to the weight of tap water contained on a board after blow off. That should directly relate to final ionic residue and water ionic content.

I do not have a scale here that is sensitive to where I can measure the difference. I hope you do.

Does ANYONE on this list have a PCB, water, air gun, oven and sensitive scale? 

Can anyone suggest a sensitive scale I can buy for not too much money? Is so I will buy one and test.

Thanks,
Bob Kondner



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Munso
Sent: Sunday, January 08, 2012 10:51 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux‏

I find it interesting that the use of tap water is still being proposed. Let's look at the residues in tap water in industrial regions. High levels of chloride, sulfate and and sodium and processing  through sand filtration creating soluble silica globules that hold concentrated pockets of contaminants.  This approached worked with rosin based fluxes in the 90s.  But lets look at the level of circuit sensitivity of today's hardware (where a half meg ohm drift will shut down a critical circuit and maybe the entire system) and the effect of residues that are moisture absorbing and conductive are creating performance problems. I propose that we run a series of evaluations comparing tap water, to RO water to DI water. Then i propose that we evaluate the results by ion chromatography using both the C3 localized extractions and bag extractions of our Umpire 2 SIR test board. Using the IPC SIR conditions of 40C/93% with continuous monitoring to assess the residue effects. Oh yes it'
 s true that the resistivity drops to nothing but not due ionic contamination that is found in tap water but the absorption of CO2 that has no residual effect on the active circuitry. Oh and if you paid attention I suggested the the board be rinsed with DI water steam and not tested in my lab so how much simpler can that be. 

Terry Munson
Foresite Inc
765-457-8095


On Jan 8, 2012, at 8:11 PM, "Robert Kondner" <[log in to unmask]> wrote:

> Before you go through the expense and effort of doing DI to clean and 
> rinse try doing a tap clean and rinse WITH a blow off cycle. Have some 
> ionic contamination tests run afterwards, they will be very clean if 
> you have a good blow off.
> 
> Washing with Di water is kind of silly, how long does Di water remain 
> DI after a wash of dirty boards start?  Maybe 100 ms? Wash with tap.
> 
> Rinse in DI might help but a blow off of tap water leaves only tiny 
> amounts of material even with very hard tap water. It really depends 
> on water entrapment issues and then even a rinse is questionable.
> 
> Try something simple and measure.
> 
> Bob K.
> 
> 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry Munson
> Sent: Saturday, January 07, 2012 7:44 PM
> To: [log in to unmask]
> Subject: Re: [TN] Cleaning water soluble flux‏
> 
> They should look at DI water steam to clean and rinse.  We have 
> effectively cleaned 2331-ZX flux. With stop steam cleaning. Call me at 765-457-8095.
> 
> Terry Munson
> Foresite
> 765-457-8095
> 
> 
> On Jan 7, 2012, at 6:36 PM, Gary Bremer <[log in to unmask]> wrote:
> 
>> I am presently working as an contractor for the next few months then 
>> back
> to unemployment, last place I worked was Jet Propulsion Laboratory on 
> the Mars Science Laboratory.  These are lighted panels for various 
> aircraft and the company policy is for J-STD-001/IPC-A-610 Class 3 The 
> failure is with miniature T-1 lamps that stop working after going through an baking process.
> Other boards that use these lamps but use RMA flux do not have this 
> problem, I suspect the cleaning process and the flux.  They do not 
> check ionic contamination and handle the boards with bare hands and 
> the operators even know when components are ESD sensitive or not.  I 
> have recommended they change the cleaning process to an Aqueous type 
> batch cleaner but this cost money which they do not wish to spend.
> Their process person believes that their process is fine and something 
> else is causing the problem (bad lamps, forming lamp leads, etc.).  This goes against all my knowledge and training.
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To 
>> unsubscribe, send a message to [log in to unmask] with following text 
>> in the BODY (NOT the subject field): SIGNOFF Technet To temporarily 
>> halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
>> per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
>> archives of previous posts at: http://listserv.ipc.org/archives For 
>> additional information, or contact Keach Sasamori at [log in to unmask] 
>> or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives For 
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
> 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 16.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2