Hi Jason
You want to first look in IPC-6012, particularly in sections Table 3-2, location specs in section 3.4.1, breakout data in 3.4.2, specs for blind/buried vias in Fig. 3-13, wrap and fill data in 3-14, and fill spec in 3.6.2.16 and more particularly in IPC 4761 which defines specifications for protection measures. Also, IPC 2221 defines via hole tolerance, and many other via plating specs.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Roetz
Sent: Wednesday, January 25, 2012 9:02 AM
To: [log in to unmask]
Subject: [TN] Via In Pad
Can anyone point me to an IPC specification that I can reference in
regards to via in pad acceptability?
Alternatively, if this does not exist, what would be acceptable criteria
for flatness, voids & dimples for VIP (filled and cap plated)?
TIA,
Jason Roetz
Master Designer
Electrical Group, Industrial Controls Division
4201 North 27th Street
Milwaukee, WI. 53216
Telephone: 414-449-6397
Fax: 414-449-7319
[log in to unmask] <mailto:[log in to unmask]>
http://www.eaton.com/ <http://www.eaton.com/>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|