Hi Richard - yes, the assessment by George and Andy fills in the gaps on
many questions we had asked. I think that it is interesting that the
parameters resulted in an optical effect. We had our "Barney boards" was a
similar case. I'll have to put this new case in my photo gallery.
Dave
"Stadem, Richard D." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/13/2012 08:27 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
Re: [TN] Strange Gold? (Analysis Done!)
I think this is an excellent report. Very interesting to see the gold
"pushed" in front of the molten solder, concentrating it. George and Andy
are to be congratulated.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, January 13, 2012 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Strange Gold? (Analysis Done!)
Hope this Friday 13th is going well for everyone,
Remember my post from back in November about the strange looking gold? The
one with the purple looking solder?
Well, I got that analyzed by one of our own Technetters; George Wenger.
Him
and his partner Andy Giamis were able to find time in their busy schedule
to
do this for me, for which I'm humbly thankful.
It's pretty interesting. Here's my original post:
..............................
Hi All,
Below is a photo of a SON8 footprint that was printed with SAC305 on a
Gold plated PCB and reflowed. I have never seen this before. Is this
"purple
plague"? If it is, exactly what causes it?
http://stevezeva.homestead.com/Strange_Gold.jpg
http://stevezeva.homestead.com/Trippy_Solder.jpg
http://stevezeva.homestead.com/Trippy_Solder_Close.jpg
Steve
..............................
I printed up one of the same panels we had the purple solder on with the
same SAC305 paste and reflowed it without parts, and got the same purple
looking solder. So I sent it to George and Andy, and here's the analysis
that they did. It's really good if you ask me.
http://stevezeva.homestead.com/FSC-5178.ppt
Steve
P.S. Thanks again George and Andy!
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|