TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 5 Jan 2012 03:46:42 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Message-ID:
Subject:
From:
Steven Creswick <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
Inge,

Sounds like Steve G will have some work to do when he gets up this morning.
Great idea to post to Steve's page.  Good ideas overall.

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Thursday, January 05, 2012 2:51 AM
To: [log in to unmask]
Subject: Re: [TN] ist report: PCB vs baking vs design

I forgot to clarify following: TechNet is under IPC, right? But I think the
name TechNet suggests that all must not necessarily be about PCBs,right?
So, my idea of share reports includes a wider perspective, all with the
purpose to make engineers being even better. Many hunger solely for the
newest and most sensational, my intention is not to ride on the edge, but
to look back and remember basics. If you don't , then  there is a risk of
repeating old mistakes again and again. At the same time I think what can I
add, the guys are so well learned and experienced already, líke Dave
Hillman, Dough Pauls, etc. On the other hand, there must be lots of guys
that do not belong to the inner circle. Those ones may appreciate some adds
to the daily meals. Widening does not mean that you must be a specialist on
everything, but to make you familiar with many topics. A CAD guy may avoid
some traps belonging to tantalums because he knows some headlines about
rush-in currents.  And a vibration operator may know what to look for if he
knows a little about cracking ceramic caps ..etc You can call it 'flags'.
Or 'bookmarks'. Right?

Allright. Bookmarks. Every each one can search themselves with a simple
googling or other crawling, so what's the meaning with my idea of a weekly
report? It's already there, together with millions of other reports. I
think, and I may be wrong, I think that people may become curious. What
will come this Friday? And they will pick the little seed and swallow.

Finally, I would rather see Dave, Dough, Trikeman, Steve Gregory or like to
do this, because they are younger and better. Why not Steve, he used to be
the operational center before.  For me, Steve is synonymous with TN. He was
the one who made me interested in TechNet.

Mission Impossible
Inge




On 4 January 2012 01:19, Inge <[log in to unmask]> wrote:

> Here is the first report, quite new facts for many, I guess, whilst
> routine for old CAD foxes.
> Key: be aware of humidity on inside of a PCB. Don't think this is  a
> simple matter, far from.
> You can even cause damage to a PCB when you think   ' let's increase the
> temperature ' , 'let's double the time'  , or other home made
> countermeasures.
>
> I send it to Steve for best way of distribution. If there is another and
> better, give advice.
>
> Ingte
>
> ______________________________**______________________________**__________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> **______________________________**__________
>
> ------------------------------**---------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/**
> archives <http://listserv.ipc.org/archives>
> For additional information, or contact Keach Sasamori at [log in to unmask]
847-615-7100
> ext.2815
> ------------------------------**-----------------------
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2