Hi all,
We've been witnessing some field failures related to cracked
capacitors. We have seen it on different PCBA's, different panel
configurations, different physical locations on boards even 3 different
capacitor suppliers. The only constant is that we always see it on the
0,1uF ceramic 0603. We've only had a couple of cross sections done as
they are relatively expensive. All cross sections done so far show
evidence of board flexing causing 45degree cracks.
There must be something along our process that causes this flexing. The
way I see it, pretty much every step can be the guilty one. From PnP,
reflow, repair, ICT, functional testing, depanelling and final
mechanical assembly...up to some extent, they could all possibly be
causing flexing and damage to capacitors. I would like to make a more
extensive study to isolate the source of our problems. Are there other
methods, less expensive than cross sectioning, to see if a capacitor is
cracked?
Have any of you faced this problem in the past? What methods did you
use to isolate the source of the problem? What were your results?
Thanks for your help,
Eric
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|