Indium had a nice paper at the last APEX on QFN outgassing vs pad design.
Here is a copy: www.kondner.com/files/qfn_voiding.pdf
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Larry Dzaugis
Sent: Tuesday, December 13, 2011 4:18 PM
To: [log in to unmask]
Subject: Re: [TN] TI Paste Recommendations
The widow pane pattern allows for the gas generated by the consumption of
the flux to escape from the thermal pad. The treatment is similar to SOD's
and QFP's with thermal pads.
On 12/13/11, Stadem, Richard D. <[log in to unmask]> wrote:
> QFNs are very typically subjected to an aperture reduction. Usually
> the peripheral pads are reduced by 10-15%, and if a large belly pad is
> present, the stencil aperture reduction is typically between 40% to
> 60% of the pad area.
>
> To understand why, think of it like this:
> A chip capacitor, resistor, or a leaded SOIC, QFP, etc. all have
> someplace for the molten solder to flow other than the pad itself.
> Chips have endcap terminations, molten solder can wet out to the edges
> of the pads and run up the sides of these endcap terminations.
> Likewise with leaded components. In all of these cases, the solder has
> somewhere to go; there is no real constraint that would cause the
> surface energy of the molten solder to go "out of bounds" in the form of
solder spattering.
>
> In the case of QFNs, if you print solder paste in a one-to-one ratio
> with the pads, the molten solder has no place to wet and flow. With
> the component body mass sitting on the resultant puddles or blobs of
> molten solder on the belly pad and the peripheral pads as well,
> spattering occurs, and that is why there are so many solder fines
> trapped under the QFN part. To prevent this, the stencil aperture is
> reduced such that the smaller amount of solder has someplace to flow.
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
> Sent: Tuesday, December 13, 2011 2:40 PM
> To: [log in to unmask]
> Subject: Re: [TN] TI Paste Recommendations
>
> For QFN, 7093 is the guideline you want. QFN is rather different
> compare to the BGAs.
>
> Joyce Koo
> Materials Researcher - Materials Interconnect Lab Research In Motion
> Limited
> Office: (519) 888-7465 79945
> Mobile: (226) 220-4760
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Bogert
> Sent: Tuesday, December 13, 2011 3:28 PM
> To: [log in to unmask]
> Subject: Re: [TN] TI Paste Recommendations
>
> December 13, 2011
>
> Solder paste size can depend on the part manufacturer recommendations.
> For example, Freescale for their BGA P013 processor recommends that
> the PC board solder pad and stencil aperture diameters should
> generally be the same; a 1 to 1 ratio.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of William Noel
> Sent: Tuesday, December 13, 2011 2:52 PM
> To: [log in to unmask]
> Subject: [TN] TI Paste Recommendations
>
> Hello all - I am working on creating a 24 pin QFN footprint for my CAD
> library. Is there a valid reason for making the solder paste smaller
> than the actual pad outline? I notice that TI consistently seems to
> recommend a smaller paste outline than pad outline. Additionally,
> they recommend a series of small square paste squares to appear on the
> thermal pad rather than a single smaller square of paste.
> Essentially, IPC-7351 recommendations are different than the TI
> recommendations. Any help? Thank you.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives For
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives For additional information, or
> contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute
> non-public information. Any use of this information by anyone other
> than the intended recipient is prohibited. If you have received this
> transmission in error, please immediately reply to the sender and
> delete this information from your system. Use, dissemination,
> distribution, or reproduction of this transmission by unintended
recipients is not authorized and may be unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives For additional information, or
> contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives For additional information, or
> contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|