Subject: | |
From: | |
Reply To: | |
Date: | Wed, 14 Dec 2011 07:47:41 -0800 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
It is possible to have the gerber soldermask layer that the fabrication house used (after they modified yours) sent to you. Then you can use a gerber comparision tool to look for differences. I agree that you want to have the final and best representation of the gerber incorporated into your library.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of William Noel
Sent: Wednesday, December 14, 2011 3:44 AM
To: [log in to unmask]
Subject: [TN] BGA SMD vs NSMD
Hello all - I am looking for some advice on building our standardized CAD models for our BGA's. I have been creating our CAD models using the IPC LP Calculator as a companion tool to the IPC-7351 SM Design and Land Pattern Standard. One of the conventions that 7351 recommends is creating solder mask shapes at a one to one size relative to the pad size. To my understanding this creates a Solder Mask Defined (SMD) solder joint. Additionally I believe this solder joint is termed a "non-collapsing" solder joint using the IPC terminology. When the solder mask is relieved by a slight amount (in other words if the opening in the solder mask is slightly bigger than the pad geometry) then this creates a Non-Solder Mask Defined (NSMD) solder joint which I believe is termed a "collapsing" solder joint using the IPC technology. Our fabrication notes indicate that the solder mask may be "swelled" by the fabrication house as appropriate to create a high quality solder joint while simultaneously insulating routes that are in close proximity to the joint itself. The concerns we have are that now the fabrication house has possibly modified our artwork and we have no way (without close examination under a microscope) of knowing if the soldermask opening was enlarged and if so by how much. We don't really want to leave it up to our designers to modify the soldermask opening for the "standardized" CAD models coming out of library. We would prefer to have our CAD model fully represent what is being built. Any advice on this subject would be appreciated. Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|