The peak temp for the electrolytic caps is measured at the top of the
cap and is warmer than the solder joint. There are other devices that
are lower than 250C max temp. Tedious, but necessary to check each
part.
Just because the oven profiled with 1 unit at these temps, doesn't
mean the oven will maintain the temperature when fully loaded. There
is no margin on the 220 location.
On 12/13/11, Leland Woodall <[log in to unmask]> wrote:
> Chris,
>
> I'd begin with the profile recommendations given by my solder paste
> supplier. Then I'd take into consideration the reflow specs for any
> temperature sensitive components, usually found to be small aluminum
> electrolytic capacitors.
>
> On a side note, if you're using SAC 305, a peak of 220 C is a bit low. This
> is barely above the melting point. Again, check the technical data sheets
> for your particular paste.
>
> Leland
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Christopher Young
> Sent: Tuesday, December 13, 2011 5:17 AM
> To: [log in to unmask]
> Subject: [TN] Thermal profile for lead free
>
> Hi all,
>
>
>
> Could you give me some data on ideal temperature against ramp time for lead
> free profile.
>
>
>
> We have a 8 zone oven with profiles as follows. Are they both ok from a
> solder process point.
>
>
>
> At reflow zone Temp is at 220 c - 240c max for 30secs on one product.
>
>
>
> Any help or thoughts on thermal profiling would be great.
>
>
>
> Regards
>
>
>
> Chris
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives For additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ________________________________
>
> “Confidentiality Notice:
> This transmission (including any attachments) may contain confidential
> information belonging to the sender and is intended only for the use of the
> party or entity to which it is addressed. If you are not the intended
> recipient, you are hereby notified that any disclosure, copying,
> distribution, retention or the taking of action in reliance on the contents
> of this transmission is strictly prohibited. If you have received this
> transmission in error, please immediately notify the sender and erase all
> information and attachments.”
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|