November 9, 2011
Is there any technical concern with hand or selective soldering a
surface mount connector with SAC387 solder tails to a CCA using Sn96
solder; both alloys melt around 221C?
Is there an technical concern with reflow or selective soldering this
connector using Sn63 solder? I am aware that there can be compatibility
issues soldering Sn63 to some SAC alloys unless the reflow soldering
profile temperature is high enough to ensure complete melting of SAC
alloy.
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------