TECHNET Archives

November 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Thu, 17 Nov 2011 14:27:06 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Message-ID:
Subject:
From:
Paul Reid <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (101 lines)
Hi Rudy,

I have found that 105°C for four hours is adequate to remove the majority of the moisture from PWBs. 

I worry that 125°C is too high for low Tg, dicey cured, product. For low end materials 125°C can reduce reliability of the board particularly if the material has a Tg of 135°C. 

Mostly 125°C is not an issue with lead/free materials but it can degrade low end materials. 

Sincerely,  
Paul Reid 
Program Coordinator  
PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario Canada, K2H 9C1 
613 596 4244 ext. 229  
Skype paul_reid_pwb 
[log in to unmask] 
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: November 17, 2011 1:12 PM
To: [log in to unmask]
Subject: Re: [TN] Recommended Bakeout Temperature for Boards and Assemblies

Rigo Garcia:  First, you are assuming that the water in the board has the same characteristics as liquid water.  It does not.  The water is chemically bonded, and needs more than 100 C to be driven off.   Second, 125 C is gentle, compared to the temperatures the board will see during soldering.

Rudy Sedlak
RD Chemical Company

--- On Thu, 11/17/11, Garcia, Rigo (GSFC-300.0)[MANTECH SRS TECHNOLOGIES] <[log in to unmask]> wrote:

From: Garcia, Rigo (GSFC-300.0)[MANTECH SRS TECHNOLOGIES] <[log in to unmask]>
Subject: [TN] Recommended Bakeout Temperature for Boards and Assemblies
To: [log in to unmask]
Date: Thursday, November 17, 2011, 8:28 AM

Good day TechNetters!

I have been reading all sorts of materials regarding bakeout of boards and the consequences. Among some of the documents I've read is IPC-1601 - "Printed Board Handling and Storage Guidelines".

One of the main questions I still have is, if moisture contributes to delamination by the internal forces generated internally on the PCB when heating up the board at high temperatures due to the evaporation of the water, why would anybody recommend temperatures above 100 °C which is the boiling temp for water? For instance, baking at 125 °C would create the same effects we are trying to avoid, wouldn't it?

Does anybody know any good reading material to learn about this?

Thanks for the help!

Rigo Garcia

Sr. Quality Assurance Engineer
Workmanship Standards, Code 300
NASA, Goddard Space Flight Center
Greenbelt, MD  20771
Phone. (301) 286-6129
Fax.       (301) 286-6576


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2