HI
Just about everyone does an RMA tacky flux.
To be classified RMA the flux has to have rosin as its major [resin]
ingredient. So if it is called RMA that must be the case. RMA doesn't mean
the tacky flux can't contain resin, in fact many do.
Just to clarify the semantics here. There are many types of resin both
natural and synthetic. Rosin is a natural resin derived from trees.
The terms resin and rosin are sometimes used interchangeably. Perhaps
because rosin was at one time the most common resin. Much as, though there
are many metal salts, we all know what we mean by "salt".
More precisely: The rosin we use is colophony or colophonium (those that
liked stickium would probably prefer this) from pine trees.
Regards
Mike
Mike Fenner
Bonding Services & Products
T: +44 [0] 1865 522 663
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dominic Boudreau
Sent: Tuesday, November 15, 2011 8:16 PM
To: [log in to unmask]
Subject: [TN] RMA rosin tacky flux
Hello Technetters, does anyone know a RMA rosin tacky flux? The question
seems simple however I've found only RMA resin tacky fluxes.
Thank you
Dominic
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|