Hafnium-Nitride has a melting point of 3310°C and Hafnium has six naturally occurring isotopes, so my vote is Hafnium, but I think somebody already mentioned Hf
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Craig Sullivan
Gesendet: Freitag, 7. Oktober 2011 14:48
An: [log in to unmask]
Betreff: Re: [TN] NTC Friday Element Quiz - the Question
Purely a guess but Tungsten is the only thing I can think of with a MP that high.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]
P Please consider the environment before printing this e-mail.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, October 07, 2011 1:11 AM
To: [log in to unmask]
Subject: [TN] NTC Friday Element Quiz - the Question
Hi folks - Here is the Friday Element Quiz Answer:
The Question:
This element is used in high temperature ceramics creating some of the most refractory materials known - an alloy using this element has a melting point of 3310C. The first pure sample of this element was made in 1925. This element has six naturally occurring isotopes. This element plays no know biological role and poses no environmental threat to plants or animals. What element is being described?
The winner of the weekly element quiz will get the services of Clumpy and Kloumpios for the week.
So far Clumpy and Kloumpios have:
Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)
Week 2 Bev Christian, RIM
- conducted REACH material testing
Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn
Week 4 Ian Fox, Goodrich
- had an epic journey of travel
Week 4 Gary Ferrari, Garrick Global
- unknown
Week 5 Fredrick Miller, Astrolab
- unknown
Week 6 David Nelson, Raytheon
- Were tackling dummys for Dallas Cowboys
Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim
Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown
Week 9 Steve Gregory of RD Circuits
- unknown
Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!
Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit
Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!
Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process
Week 14 Bev Christian, RIM
- assisted with a tin pest investigation/test
Week 15 Bev Christian, RIM
- assisted Bev shoveling snow
Week 16 David Bealer of Watchfire Signs
- assisted with reflow profiling
Week 17 Brian Ellis, rumored to be retired
- assisted with rewiring the house, had a tractor accident and found his cousin Kloumpios
Week 18 Denny Fritz, SAIC
- assisted with tin whisker inspection/examinations
Week 19 Graham Collins, L3 Communications
- assisted with scraping barnacles, boat paint and boat engine maintenance
Week 20 Mark Woolley, PTRL Laboratory Avaya
- assisted with weather observations (70F to snow) and resolving electrochemical migration failures
Week 20 Tom Carroll, Boeing Defense, Space and Security
- assisted with commercial aircraft galley inspection
Week 21 Brian Ellis, supposedly retired, and Tom Carroll, Boeing Defense, Space and Security
- assisted with root cause corrective action tasks
- assisted with nothing but catching up with the family
Week 22 Drew Meyer, Benchmark Electronics Inc.
- assisted with metallographic cross-sections and Dye & Pry testing
Week 23 Bev Christian, RIM
- assisted with a creep corrosion project and the setting up of an oxygen bomb
Week 24 Steve Gregory, RD Circuits
- unknown
Week 25 Ahne Oosterhof, A-Laser
- assisted with stencil aperture data analysis and split/stacked firewood
Week 26 Scott Post, Delphi
- assisted/participated in the Kokomo Airshow Race Event
Week 27 Brian Ellis, supposedly retired
- assisted with tedious website work and family home cooking
Week 28 Nigel Burtt
- abandoned Nigel and were rumored to be involved in UK News Corps/News International cellphone/journalism/politics scandal
Week 29 Richard Stadem,GD-AIS
- unknown
Week 30 Robert Wolfe, Kimchuk Inc and Graham Naisbitt, Gen3
- assisted with a hot tub refurbishment for post work day de-stressing
- assisted with SIR and Cleanliness testing
Week 31 Bev Christian, RIM Inc, and Denny Fritz, SAIC
- assisted with lab testing
- assisted with tin whisker investigations
Week 32 Steve Mikell, supposedly retired
- attempted to provide both US Congress and EU lawmakers "engineered"
solutions
Week 33 Mark Woolley, PTRL Laboratory Avaya
- unknown
Week 34 Leland Woodall, CSTech Inc.
- assisted with new model qualifications,updating supporting documentation, strain gaging, performing cross sections, verifying a new selective soldering process, and finally assisted with the development of a plant-wide countermeasure effectiveness auditing program (Wow, they had to work hard this week!)
Week 35 Joe Russeau, Precision Analytical Laboratories
- assisted with new equipment preparations
Week 36 Patrick Goodyear, PGE
- assisted with beach trash collection duty
Week 37 Dave Elder, Tait Radio Communications
- assisted Dave Hillman with a geography lesson, watch USA vs Irland in World Rugby Cup and went skiing.
Week 38 Steve Mikell, supposedly retired
- assisted with ????
Week 39 Andy Giamis, Commscope
- assisted with metallographic cross-sectional analysis of die cast Mg and taught a group of Cub Scouts how to hotwire a tractor
Week 40 ????
- assisted with ????
Everyone have a safe weekend.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the property of MPL Incorporated, intended only for the use of the intended recipient(s). Unauthorized use or disclosure of this information is prohibited. If you are not an intended recipient, please immediately notify MPL Incorporated and destroy any copies of this email. Receipt of this e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain information that is company confidential or privileged. Any technical data in this message may be exported only in accordance with the U.S. International Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use is strictly prohibited and may be unlawful. If you are not the intended recipient, or the person responsible for delivering to the intended recipient, you should not read, copy, disclose or otherwise use this message. If you have received this email in error, please delete it, and advise the sender immediately.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
**************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. ****************************************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|