TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dennis Fritz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dennis Fritz <[log in to unmask]>
Date:
Mon, 31 Oct 2011 12:49:01 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (174 lines)
Steve, 

Sorry, I missed the tin plated finish on the connectors.  They almost certainly are electroplated connectors, whereas the Continental parts were immersion plated circuit boards. However, both immersion and electroplated tin have been shown to grow tin whiskers.  

Yes, there is concern for tin whiskers in your case.  The most likely spot is where the compression stress is highest.  That said, what can be done?  I think your connector spacings are large - some "rule of thumb" designs get nervous about tin whisker shorts at spacings of 500 microns (20 mils) or less. JEDEC specs on whisker inspection call out whisker problems at 50 and 67 microns  - 2 to 2.5 mils, but that is on parts that have been accelerated only a matter of 1.5 to 4 months. The expectation is that tin whiskers will continue to grow over time for the components that start showing whiskers shortly after manufacture. 

Finally, you ask about whiskers that break off and move around. That is Foreign Object Debris - FOD.  Moving tin whiskers can cause shorts, the same as zinc whiskers from the computer room galvanized floor supports can re-circulate in the computer room air handling system and land on/short out computer boards in servers, etc.  Conformal coating is one prevention for FOD shorts.

Denny



-----Original Message-----
From: Steve Gregory <[log in to unmask]>
To: 'Dennis Fritz' <[log in to unmask]>; TechNet <[log in to unmask]>
Sent: Mon, Oct 31, 2011 12:06 pm
Subject: RE: [TN] Whiskers from Immersion Tin Finish?



Hi Denny,
 
Oh but they are tin plated, it says so on the datasheet. I’m a little concerned that stress seems to encourage whisker growth on tin plated components.
 
These contacts are crimped on the end of a wire, wouldn’t that be a stress to be concerned about? Granted, these contacts get inserted into a plastic shell, but where do the whiskers go when they break off from the contacts?
 
Steve
 

From: Dennis Fritz [mailto:[log in to unmask]] 
Sent: Monday, October 31, 2011 11:55 AM
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] Whiskers from Immersion Tin Finish?

 


Guess I should have been a bit more clear about "press fit connections".   What Continental had was circuit boards with immersion tin finish, and they inserted press fit pins into those.  Where the press fit portion of the pin entered the plated through hole, whiskers grew out of the hole and I think from the corners of the hole.   Continental tried a number of pin configurations - "eye of the needle", and several more ways to get the gas tight fit in the hole - and as I remember, some difference in whiskering based on pin configuration. 

 

I am talking more about this technology:

http://www.interplex.com/compliant/pressfit

 

I don't think the pins/sockets you show here would be tin plated and I don't see how they are pressed into the board. 

 

Denny

-----Original Message-----
From: Steve Gregory <[log in to unmask]>
To: 'TechNet E-Mail Forum' <[log in to unmask]>; 'Dennis Fritz' <[log in to unmask]>
Sent: Mon, Oct 31, 2011 8:49 am
Subject: RE: [TN] Whiskers from Immersion Tin Finish?

Hi Denny,
 
So, if I were to be building a wire harness with a tin plated Samtec contact
( http://www.samtec.com/documents/webfiles/cpdf/CC69X-XXXX-01-X-XX-MKT.pdf
), I should be concerned?
 
Steve
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Monday, October 31, 2011 8:15 AM
To: [log in to unmask]
Subject: Re: [TN] Whiskers from Immersion Tin Finish?
 
Continental Electronics presented a paper at the IPC Whiskers seminar in
Schaumburg, IL concerning press fit connectors using immersion tin.  Seems
the extreme compression exerted by the press fit operation can really cause
whiskers to grow from immersion tin plated boards. I think they uncovered
the problem by examining a filed failure of an automotive electronics
module.  Seems to me that on one occasion, even after they potted and cross
sectioned a connector, a tin whisker grew out of the surface of the cross
section from the immersion tin in/near the through hole in the board.  Now
that's some long lasting compressive stress. 
 
Denny Fritz
 
 
 
 
 
 
 
 
-----Original Message-----
From: Jack Olson <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Fri, Oct 28, 2011 4:20 pm
Subject: [TN] Whiskers from Immersion Tin Finish?
 
 
I've always been under the impression that the risk of Tin Whiskers was
ostly from the portion of component leads that don't get wetted with
older. (for example, a right-angle through hole connector may have exposed
eads ABOVE the solder joint area)
Now I'm being asked about the risk of whiskers from Immersion Tin finish in
reas that don't get soldered, like vias, or lands of components that don't
et populated. I haven't heard any of you talking about that, is this a
isk?
My first response was "naw, don't worry about it..",
ut then I turned to IPC-4554 and see a whole section (3.9) on "Whisker
ssues"
ith Tables
nd Beautiful Photographs
nd advice on Measuring them,
nd methods of Rating them,
nd on and on...
SERIOUSLY?
(sigh)
Jack
 
_____________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask] 
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 16.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
or additional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------
 
 
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
 
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
 




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2