We had "Greenies". Everclear and green crème de menthe.
Dewey
-----Original Message-----.
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, October 31, 2011 9:03 AM
To: [log in to unmask]
Subject: Re: [TN] Rookie question on RMA fluxes
YEE-HAW! Everclear! I remember a concoction we used to call "Purple Jesus"
with Everclear that we partied on when I was younger (lots younger)...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Monday, October 31, 2011 11:44 AM
To: [log in to unmask]
Subject: Re: [TN] Rookie question on RMA fluxes
I use alcohol on a regular basis to clean fluxes, but it is NOT IPA, I use
only pure Ethyl "grain" alcohol undenatured 200 proof (this stuff is food
grade) It can be a little expensive and you have to pay the state and
federal taxes on it, but as a cleaner it is fantastic. There a very few
problems with it, it will craze some polycarbonates but one just has to be
careful. The other drawback is you have to use it in a VERY WELL
VENTILATED room as you will not be able to drive after you use it in an
enclosed area for a prolonged period, you may not even be able to walk.
pat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Friday, October 28, 2011 9:42 AM
To: [log in to unmask]
Subject: Re: [TN] Rookie question on RMA fluxes
Technos,
Once again, thanks for the inputs. The funny part is, it seems that RMAs are
still in demand in my corner of the planet, which is, guess what, the home
of the Montreal protocol.
BTW, the alcohol cleaning of the RMA is something that was humming around my
brain, as I was sure having heard somewhere that this is the solvent for RMA
residues. Good thing I've asked.
While you folks were considering my question, I've looked up RMA in Wassink
and B. N. Ellis and MacLeod Ross' books, with not much success in finding
specific cleaning methods, so it became kinda clear for me that this type of
flux is not different from the rest, cleaning wise.
Anyways, I shalt get ready for the challenge.
Best regards,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T |
450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W |
www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
De : [log in to unmask] [mailto:[log in to unmask]]
Envoyé : October-28-11 12:28 PM
À : TechNet E-Mail Forum; Ioan Tempea
Objet : Re: [TN] Rookie question on RMA fluxes
Ioan,
You have gotten a lot of good answers to the question so far and I will chip
in my two cents worth.
Technically, there is no such thing as an RMA flux anymore, though the term
continues in use. RMA, Rosin Mildly Activated, was a flux terminology from
the good old days of MIL-F-14256, the military flux specification. It was
cancelled in 1995 and directed people to J-STD-004, the current predominant
flux specification in the industry. The older rosin flux formulations that
were termed RMAs, translated into ROL0, ROL1, or ROM0, depending on the flux
and who you ask. RMA fluxes are still available, though as the market
shrinks for these, they are becoming more expensive, which encourages users
to transition to something more modern.
Most people still using "RMA" flux are using the 15% solids, which is still
pretty high, compared to low residue fluxes or water soluble fluxes. Which
means there is a significant amount of flux to clean off compared to other
fluxes.
Isopropyl alcohol sucks as a cleaner, at least in my opinion. People want
to use it because it is cheap, available almost everywhere, does not impact
industrial emissions much depending on where you are in the world, and is
not a health hazard, if you don't get too wrapped around the axle over
flammability. No way, no how would I ever want to clean an RMA flux with
alcohol alone. Does not work reliably.
In my experience, high solids rosin fluxes tend to be OK if you leave them
alone, or if you totally remove them. If you "kind of" remove them, you
have a great deal of problems. You remove the encapsulating effect of the
rosin (which you want), but you free up the activators to cause havoc (which
you don't want). In my view, you want a really effective heated saponifier
in an in-line aqueous cleaner, with a thorough heated deionized water rinse.
Doug Pauls
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/28/2011 08:07 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
[TN] Rookie question on RMA fluxes
Dear Technos,
Although I've been around in this trade of ours for quite a while now, I
have never had the occasion to work with RMA fluxes. I need to know how this
functions. How can RMA be cleaned, I've heard about alcohol...? Is regular
aqueous wash enough? If alcohol only, do we need a special equipment?
Anything else to know?
And, anyways, are RMA fluxes still available?
Also, I imagine most of you at ease with RMA have tried to talk your
customers into converting to water soluble flux chemistries. How hard was
that? Is it possible?
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]>
W | www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|