TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 24 Oct 2011 08:01:43 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Message-ID:
Subject:
From:
Ioan Tempea <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (141 lines)
Victor,

No repairs, straight from the line, can't figure out if any touch ups were done in the area, though. No golden fingers on this board and the phenomenon is always located pretty much in the same area, near the brown connector you seen at the right of the first slide.
I wonder if there is something related to the connector, as Inge suggests?

Thanks,

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] 
W | www.digico.cc

N'imprimer que si nécessaire - Print only if you must


-----Message d'origine-----
De : Victor Hernandez [mailto:[log in to unmask]] 
Envoyé : October-22-11 10:39 AM
À : [log in to unmask]
Objet : Re: [TN] Discoloration on plated over vias

Are these boards that have been reworked/repaired or straight from the assembly line?   How many boards exhibit this anomaly?   What is the appearance of the gold fingers?

"X"

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Saturday, October 22, 2011 9:31 AM
To: [log in to unmask]
Subject: Re: [TN] Discoloration on plated over vias

l'oeil est fraudé ? Peut-être. I believe something is bleeding out from the
adjacent components. Check if there are any more sites with exactly the same
parts, but with no discoloration. If the answer is negative, I think even
stronger, that the issue is connected with the two packages.

seulement une proposition

Inge
On 21 October 2011 22:26, Ioan Tempea <[log in to unmask]> wrote:

> Dear Technos and Smarts,
> I got this issue, see 

http://ipc-technet.groupsite.com/gallery/21662
>
> So 6 layer, 2oz Cu per layer PCB, epoxy filled vias and plated over. After
> assembly we see 4-5 vias having reddish stains, on most boards. Had it
> analyzed, no trouble with via integrity, no cracks in cover plating, no
> migration of fluids from inside out. FTIR does not detect any surface
> contamination.
>
> Au plating thickness stands at 2.09 micro inches.
>
> Nothing special detected in the stains, so the lab concluded what we see is
> an optical effect due to a certain roughness of the Cu. The logical
> conclusion is no issue, cosmetic defect.
>
> However, our end customer, high reliability, want to know what the stains
> are and want absolute confirmation that long term reliability is not
> affected. Also, we've been warned that no such issues will be tolerated on
> future lots.
>
> My questions to your infinite knowledge is: have you seen this before? How
> can I convince the customer everything is OK? What is the root cause and how
> can I get rid of the issue?

> Many thanks,
>
> Ioan Tempea, ing.
> Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
> T | 450.967.7100 ext.244
> E | [log in to unmask] <mailto:[log in to unmask]>
> W | www.digico.cc <http://www.digico.cc/>
>
>  N'imprimer que si nécessaire - Print only if you must
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2