We are trying to identify the root cause of an issue with the tuning of an RF circuit on FR-4 laminate. We are seeing a major shift in the attenuation of the received signal from room temperature (~20 deg. C) to high operating temperature (~60 deg. C). I know that the volume and surface resistivity of FR-4 (GF/GFN) can change by a factor of up to 10^2 over the working temperature range of the laminate. Does this shift in performance also track with the dielectric constant and loss tangent of the material? If so does anyone have documentation as to how these properties change over working temperature?
Thanks for any input.
Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle
Systems Development Engineering Services
505 King Ave
Columbus Ohio 43201-2693
Phone (614)424-7582
[cid:[log in to unmask]]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|